Recently, a customer asked: What should be done about flow marks on injection-molded ABS glossy panels?
A small suggestion:
1、Check whether a highlight masterbatch was used (our highlight masterbatch has improved flowability);
2、It is recommended to increase the mold temperature to [70-80℃];
3、Use [high speed and high pressure] for injection.
(If the problem persists, you are welcome to send us a sample for analysis!)